File:Cast iron tensile test.JPG

Original file(861 × 1,200 pixels, file size: 427 KB, MIME type: image/jpeg)

Commons-logo.svg This is a file from the Wikimedia Commons. The description on its description page there is shown below.
Commons is a freely licensed media file repository. You can help.

Summary

Description Fractured tensile test specimen of a nodular graphite cast iron. This specimens failed by brittle failure, as seen from the lack of plastic deformation. Note that nodular graphite cast irons are usually ductile, so this specimen is not representative for this class of alloys.
Source Own work
Author Sigmund

Licensing

I, the copyright holder of this work, hereby publish it under the following licenses:
w:en:Creative Commons
attribution share alike
This file is licensed under the Creative Commons Attribution-Share Alike 3.0 Unported license.
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
  • share alike – If you remix, transform, or build upon the material, you must distribute your contributions under the same or compatible license as the original.
GNU head Permission is granted to copy, distribute and/or modify this document under the terms of the GNU Free Documentation License, Version 1.2 or any later version published by the Free Software Foundation; with no Invariant Sections, no Front-Cover Texts, and no Back-Cover Texts. A copy of the license is included in the section entitled GNU Free Documentation License.
You may select the license of your choice.

Captions

Example of a brittle fracture of cast iron specimen, after tensile testing

Items portrayed in this file

depicts

image/jpeg

6452215e6375f314486d1f6b4c64d40dfccfdc9f

437,432 byte

1,200 pixel

861 pixel

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeDimensionsUserComment
current04:01, 21 July 2009861 × 1,200 (427 KB)Sigmund419{{Information |Description=Tensile test specimen of a nodular graphite cast iron. Typical brittle fracture appearance. |Source=self-made |Date= |Author= Sigmund |Permission= |other_versions= }}